Tungsten carbide is brazed with 40Cr medium carbon steel using vacuum brazing technology. Vacuum brazing method is suitable for mass production of various tungsten carbide cutting teeth for drilling. It can complete the brazing of multi-blade carbide tools in one heating, with high brazing efficiency. Previously, most carbide tools were embedded in medium carbon steel or low-alloy steel matrix using welding methods. The welding process is closely related to the performance of the carbide, and the quality of the welding directly affects the effectiveness of the carbide’s use. When vacuum brazing tungsten-cobalt-titanium carbide, it is necessary to minimize the residual welding stress. Measures must be taken to reduce brazing stress during welding, such as reducing brazing temperature, preheating and slow cooling before welding, selecting brazing materials with good plasticity, adding compensating shims, and improving joint structures. When brazing large-area carbides, regardless of their high or low strength, special measures should be taken to reduce welding stress and prevent crack formation.

How to Vacuum Braze Tungsten Carbide?Coal Cutting Teeth? 2

Selection of carbide?Brazing Materials

The brazing materials for tungsten carbide and steel brazing are divided into three categories: high-temperature brazing materials, room-temperature brazing materials, and low-temperature brazing materials according to their melting points and brazing temperatures.

High-temperature Brazing Materials

Brazing materials with a brazing temperature above 1000°C are called high-temperature brazing materials, such as purple copper and 106 brazing materials, etc. Medium-temperature brazing materials have a brazing temperature between 850 and 1000°C, such as H62 and H68 brass brazing materials, etc. Low-temperature brazing materials refer to brazing materials with a brazing temperature between 650 and 850°C, such as B-Ag-1 and L-Ag-49 silver-containing brazing materials.

Room-temperature Brazing Materials

Purple copper brazing materials have a high brazing temperature and low weld seam strength, and are mostly used for vacuum brazing. Pure copper brazing materials have a single-phase structure, are relatively easy to control the brazing temperature, have good wetting ability for various types of carbides, good plasticity, and are the cheapest. The shear stress of purple copper brazing weld seam is about 150MPa, and it can be used below 400°C. The brazing temperature of H68 brass is much lower than that of purple copper, but because of its low weld seam strength, it is not commonly used. The melting point and brazing temperature of H62 brass are relatively low, and the weld seam has certain room temperature strength, making it a commonly used carbide?brazing material. It is generally used for carbide?tools under medium and small loads. When high temperature strength of the weld seam or small welding area is required, 105 brazing material should be used.

Low-temperature Brazing Materials

L-Ag-49 low-temperature silver brazing material is widely used abroad because of its low melting point (690-710°C), good wetting ability for tungsten carbides, and advantages such as convenient brazing and low stress. When necessary, purple copper sheets can be used as compensating shims, which can almost completely eliminate brazing stress and prevent brazing cracks. It can be used for brazing some easily cracked carbides or some large brazing surface carbide tools. Since the workpiece brazed with L-Ag-49 silver brazing material will rapidly decrease in weld seam strength as the operating temperature increases, the working temperature of the workpiece brazed with L-Ag-49 brazing material should be limited to below 200°C. The brazing fluxes used in conjunction with L-Ag-49 brazing materials contain more fluorides and chlorides, requiring higher cleaning requirements after welding, otherwise, surface corrosion of the workpiece may occur due to inadequate cleaning.

Ultra-low-temperature Brazing Materials

B-Ag-1 brazing material is an ultra-low-temperature silver brazing material with a melting point around 600-610°C, which can further reduce the residual stress of tungsten carbide joint and can also be used for brazing some easily cracked workpieces with purple copper sheets as compensating shims. Due to the ultra-low melting point of B-Ag-1 silver brazing material and its good wetting ability to tungsten carbide, it is also suitable for brazing certain diamond tools such as large diamond saw blades. However, the price of B-Ag-1 silver brazing material is high, and its high-temperature strength is low, so it is only suitable for use at temperatures below 150°C. The cadmium content in this brazing material is 24%, which is easy to evaporate at high brazing temperatures, harmful to human health. In addition to controlling the brazing temperature during brazing, exhaust devices should also be installed at the brazing operation site. After brazing, attention should also be paid to cleaning the workpiece thoroughly to prevent corrosion of the workpiece.

How to Vacuum Braze Tungsten Carbide?Coal Cutting Teeth? 3

 

Selection of Brazing Flux

The function of brazing flux is to reduce the oxides on the surface of the shank and tungsten carbide, enabling the brazing material to wet the metal surface to be brazed effectively. Generally, the melting point of brazing flux is at least 100°C lower than that of the brazing material, with good fluidity and low viscosity. The melted brazing flux during brazing serves to protect the brazing material and brazing surface, while also acting to reduce oxides.

The main requirements for carbide?brazing flux are as follows:

1.The flux should exhibit good wetting ability on both the carbide?to be brazed and the steel substrate, ensuring that it possesses good fluidity and penetrability.

2.One of the characteristics of carbide?use is its high red hardness, so it’s crucial to ensure that the brazed weld seam has sufficient strength at both room temperature and high temperatures.

3.The melting point of the flux should be as low as possible to minimize brazing stress and prevent cracking. However, the melting point of the flux should be at least 300°C higher than the working temperature of the weld seam to ensure that the tool can function normally at high cutting speeds.

4.The flux should not contain elements with low evaporation points to avoid affecting joint quality during brazing heating or posing health risks.

 

Preparation Before Vacuum Brazing

1.Prior to vacuum brazing, check whether the tungsten carbide has cracks, bends, or uneven surfaces. The brazing surface must be flat. If the brazing surface is spherical or rectangular, it should conform to certain geometric shapes to ensure good contact between the alloy and the substrate, thus guaranteeing brazing quality.

2.Perform sandblasting treatment on the carbide. If sandblasting equipment is not available, the oxide layer and black grade letters on the brazing surface can be removed by holding the tungsten carbide by hand and grinding it on a rotating green silicon carbide wheel. If the oxide layer on the brazing surface of the carbide is not removed, the brazing material will not wet the carbide easily. It has been verified that if there is an oxide layer or black grade letters on the brazing surface, sandblasting treatment should be carried out. Otherwise, the brazing material will not wet the carbide easily, and black letters will still appear in the brazing seam, reducing the brazing area and causing brazing defects.

3.When cleaning the brazing surface of the carbide, it is best not to use chemical mechanical grinding or electrochemical grinding methods. Instead, wire cutting by electric spark erosion should be used. The processed tungsten carbide can then be sandblasted again or ground with a green silicon carbide wheel to remove the surface layer. The sandblasted carbide can be cleaned with gasoline or alcohol to remove oil stains.

4.Before vacuum brazing, carefully check whether the groove shape on the steel substrate is reasonable, especially for carbide grades prone to cracking and tungsten carbide workpieces with large brazing surfaces. Stricter requirements should be imposed. The grooves should also be sandblasted and cleaned to remove oil stains. When the cleaning volume is large, an alkaline solution can be boiled for 10-15 minutes. For multi-blade tools and complex gauges brazed with high frequency or immersed copper, it is best to boil them in a saturated borax water solution for 20-30 minutes, take them out to dry, and then carry out welding.

5.Before using the brazing material, wipe it clean with alcohol or gasoline and cut it into shape according to the brazing surface. When brazing general carbide cutting tools or molds, a brazing material thickness of about 0.4-0.5mm is suitable, and its size should be similar to the brazing surface. When using continuous nitrogen protection for brazing furnace heating, the brazing material can be appropriately increased. When brazing tungsten carbide multi-blade cutting tools, gauges, etc., the brazing area should be minimized. Generally, the brazing material can be cut to about 1/2 of the brazing surface. When the brazing technology is proficient, the brazing material can be reduced to 1/3 of the brazing surface or even smaller. Reducing the amount of brazing material can make the appearance of the welded workpiece more beautiful and facilitate grinding.

tungsten carbide teeth braze method

Vacuum Brazing Process

Uniform Heating of the Shank and carbide Inserts The correct vacuum brazing process for tungsten carbide tools plays a crucial role in welding quality. The heating rate significantly affects the quality of the weld. Rapid heating can cause cracks and uneven temperatures in the carbide inserts. However, heating too slowly can lead to surface oxidation, reducing joint strength.

During vacuum brazing of carbide tools, uniform heating of the shank and carbide inserts is one of the basic conditions to ensure welding quality. If the temperature of the tungsten carbide inserts is higher than that of the shank, the melted brazing material wets the carbide inserts but not the shank, leading to decreased joint strength. In this case, when shearing the alloy insert along the weld layer, the brazing material remains intact, detaching along with the alloy insert. Milling marks from the shank support surface can also be seen on the weld layer. Conversely, if the heating rate is too fast and the temperature of the shank is higher than that of the alloy inserts, the opposite phenomenon occurs.

Arrangement of Flux, Brazing Material, and tungsten carbide Inserts

The sequence and positions of flux, brazing material, and carbide inserts directly affect brazing quality. The correct arrangement method is as follows: place the brazing material on the groove, sprinkle flux, then place the carbide inserts, and sprinkle another layer of flux along the side weld seam on the top surface of the carbide inserts. This facilitates temperature control during brazing, reducing excess brazing material adhering outside the weld seam. It’s crucial to control the vacuum brazing temperature of the workpiece correctly. Excessive vacuum brazing temperature can cause weld seam oxidation and zinc evaporation from zinc-containing brazing materials.

Brazing Parameters

During vacuum brazing, maintain a vacuum degree of about 5 X 10-2 Pa. The heating rate is an important parameter during vacuum brazing, as excessive heating rate leads to a sharp drop in vacuum degree, which can cause oxidation of carbide and brazing materials. In production, the vacuum brazing process is as follows: increase the temperature from room temperature to 800°C at a rate of 10°C/min, hold for 30 minutes, then increase the temperature to the set temperature at a rate of 9°C/min, hold for 10 minutes, and then cool down with the furnace. The 800°C holding temperature ensures uniform heating of the base material. Increasing the temperature to the set temperature at a rate of 9°C/min ensures that the vacuum degree does not decrease significantly, and the short-term holding at the set temperature allows the brazing material to melt fully and prevents excessive evaporation of particulate magnesium in high vacuum.

Cooling Speed After Vacuum Brazing

The cooling speed after vacuum brazing is one of the main factors affecting brazing cracks. During cooling, instantaneous tensile stress occurs on the surface of carbide?inserts, and the tensile stress of carbide?is much lower than the compressive stress. Especially for carbide?grades such as YT60, YT30, and YG3X, which have large brazing areas and small matrices but large carbide?inserts, attention should be paid to the cooling speed after brazing. Usually, the post-welded workpiece is immediately immersed in lime or charcoal powder to cool slowly. This method is simple but does not control the tempering temperature. If conditions permit, the workpiece can be immediately placed in a furnace at 220-250°C for tempering for 6-8 hours after brazing. Low-temperature tempering can eliminate some brazing stress, reduce cracks, and prolong the service life of carbide?tools.

Cleaning After Vacuum Brazing

After vacuum brazing, the product can be polished with sandpaper and then polished with polishing paste. Post-brazing cleaning of well-brazed carbide?parts is necessary to remove residual flux around the weld seam. Otherwise, excess flux will clog the grinding wheel during tool sharpening, making grinding difficult. Residual flux after brazing can also corrode the weld seam and base material. Common cleaning methods include boiling the cooled workpiece in boiling water for about 1-2 hours, followed by sandblasting to remove residual flux and oxides adhering to the weld seam surroundings. Alternatively, the workpiece can be immersed in an acid bath for pickling (nitric acid concentration of 3%-5%) and washed with NaOH solution. The pickling time is about 1-4 minutes, followed by thorough rinsing in cold and hot water tanks.

 

Quality Inspection of Vacuum Brazed Products

The main inspection focuses on the quality of the brazed joint between the carbide?and the steel shank, as well as the presence of cracks in the carbide. A normal weld seam should be uniform without black spots, and the unfilled portion of the weld seam should not exceed 10% of the total length of the weld seam. The width of the weld seam should be less than 0.15mm. If the brazed blade is skewed and does not meet the drawing requirements, it should be re-brazed. The tendency for cracks in carbide?blades can be checked using the following methods:

1.After cleaning the tool with sandblasting, wash it with kerosene and then observe it with the naked eye or a magnifying glass. When there are cracks on the blade, obvious black lines will appear on the surface.

2.Prepare a solution by mixing 65% kerosene, 30% transformer oil, and 5% pine oil, and add a small amount of Sudan red. Immerse the pre-checked tools in this solution for about 10-15 minutes, then remove and rinse them with clean water. Apply a layer of kaolin clay, dry it, and then inspect the surface. If there are cracks on the tool, the color of the solution will be displayed on the white clay, which can be clearly seen with the naked eye.

 

Resumen

The characteristics of using carbide?tools in mining are large impact loads and vibrations, requiring the carbide?inserts to be firmly brazed with minimal brazing stress. The surface roughness of groove machining has a significant impact on the strength of the weld seam. The lower the roughness, the higher the strength of the weld seam (although lower roughness makes machining more difficult). Generally, a roughness of around Ra6.3 is sufficient. To obtain weld seams that are thin and uniform in appearance, the groove machining accuracy of carbide?gauges should be higher.

In conclusion, the vacuum brazing and quenching of cutter teeth are becoming increasingly common due to their high production efficiency, stable quality of brazed joints, and complete heating, brazing, and quenching in a vacuum environment, which avoids oxidation and decarburization of the cutter teeth. Therefore, the vacuum brazing and quenching process for cutter teeth will be more widely adopted.

Deja una respuesta

Tu dirección de correo electrónico no será publicada. Los campos obligatorios están marcados con *

日本成熟人妻在线看片-亚洲国语精品激情在线-欧美性生活之欧美日韩-成人黄色av在线观看| 九九热在线视频精品一-国产乱码精品一区二区蜜臀-乱妇乱熟女妇熟女网站视频-国产精品午夜视频在线| 在线看片国产福利你懂得-av中文字幕精品一本久久中文字-亚洲一区二区三在线高清真人-日韩在线不卡视频免费看| 久热在线视频精品99-国产欧美日韩久久午夜-在线观看亚洲精品91-黄色大片一区二区久久精品视频| 开心五月这里只有精品-欧美日韩国产亚洲中文高-玩弄漂亮邻居少妇高潮-av资源中文在线天堂| 国产欧美日韩精品一区二-久久精品国产精品青草色艺-人妻熟妇视频一区二区不卡-亚洲国产精品第二在线播放| 一区二区在线观看黑人-久久久精品人妻一区二区三区综合-成人内射国产免费观看-四虎在线免费视频观看| 亚洲香蕉久久一区二区三区四区-国产夫妻内射一级一片-成人午夜福利片免费观看-一区二区三区四区黄色网| 国产高清丝袜av综合-精品亚洲一区二区在线-国产丝袜大长腿精品丝袜美女-日本熟女午夜福利视频| 人妻精品一区二区视频免费-99热视频免费在线观看-亚洲av第一第二第三-乱码人妻精品一区二区三区| 97中文字幕一区二区三区-国产精品亚洲av无人-亚洲国产精品自产拍久久-成人深夜福利在线视频| 九九热在线免费视频播放-久久综合九色综合久久久-国产粉嫩小仙女裸体区一区二-中文字幕巨乳人妻在线| 国产精品自拍射精视频-蜜桃视频在线中文字幕-黑人泄欲一区二区三区-国内少妇无套内射精品视频| 久99久热这里只有精品-日韩av一区二区三区播放-天堂日韩av在线播放-中文字幕被侵犯的人妻| 午夜精品久久内射电影-亚洲精品自拍视频免费在线-国产免费观看久久黄av麻豆-麻豆国产精品伦理视频| 极品美女色诱视频在线-欧美久久天天综合香蕉伊-久久精品人人澡夜夜澡-亚洲一区二区三区四区伦理| 四虎永久在线精品免费青青-久久久久久久 国内精品-国产精品四虎永久免费视频-男人天堂av免费观看| 日本淫片一区二区三区-精品亚洲人伦一区二区三区-精品成人短视频在线观看-日韩亚州欧美国产另类| 国产精品视频午夜福利-一本大道久久综合一区-成年深夜福利在线观看-国产传媒免费在线视频| 蜜臀av午夜精品福利-日韩精品av在线一区二区-丰满熟女人妻一区二区三区-懂色日韩欧美国产亚洲| 亚州国产精品一区二区-尤物在线观看视频免费-国产91久久精品视频-一色桃子中出欲求不满人妻| 欧美日韩精品视频免费下载-中文字幕一区二区三区伦理-一级特黄大片亚洲高清-午夜欧美日韩精品久久久久| 国产成人高清视频在线观看免费-人妻精品一区二区在线视频-国产成人一区二区三区精品久久-农村肥白老熟妇20p| 亚州一区二区五码在线观看-97在线视频免费公开-小明久久国内精品自线-人妻av天堂综合一区| 久草免费福利在线播放-女同女同恋久久级三级-亚洲中文字母在线播放-91精品国产麻豆国产自产在| 尤物视频在线观看网址-欧美午夜精品久久福利-久久这里只有精品视频5-国产精品成人综合色区| 国产黄片一区二区在线-国产精品99国产精品久久-国产,欧美视频免费看-长腿丝袜国产在线观看| 亚洲免费看三级黄网站-日韩国产熟女免费精品老熟女视频-久青草视频免费在线播放-国产日韩精品久久一区二区| 欧美高清视频在线高清观看-四虎最新在线播放视频-亚洲中文字幕永久在线全国-亚洲国产av成人精品成人| 日韩午夜精品免费视频-真实国产精品自拍视频-91麻豆精产国品一二区灌醉-一本色道久久综合亚洲精品东京热| 欧美性色婷婷久久久精品-久久这里只有精品国产宅男av-久久男女爱爱视频免费观看-另类福利亚洲丝袜激情在线| 91精品在线播放黑丝后入-97免费在线播放视频-av网站天堂网国产av-亚洲熟妇乱色一区二区三区| 亚洲国产高清一区二区三区不卡-亚洲综合小综合中文字幕-亚洲黄色成人av在线-日韩一区二区三区av观看| 四虎永久在线高清国产精品-一区二区三区日本精品视频-国产午夜福利精品久久不卡-一区二区三区国产亚洲自拍| 蜜桃臀欧美日韩国产精品-最近欧美日韩一区二区-亚洲综合成人一区二区三区-免费五十路熟妇在线视频| 精品少妇人妻av蜜桃-成年人网站在线免费播放不卡-免费黄色片成人国产精品-蜜桃中文字幕在线视频| 日韩视频精品在线播放-国产91亚洲精品久久-亚欧洲乱码视频在线观看-亚洲国产成人91精品| 精品国产精品久久一区免费式-男女高清无遮挡免费视频-av男人的天堂一区二区三区-免费观看视频网站97| 久久噜噜噜精品国产亚洲综合-91精品国产高清久久福利-精品国产一区二区三区麻豆-日本加勒比一区二区在线观看免费| 国产精品免费av一区二区-91在线日本在线观看-免费在线激情视频网址-亚洲午夜福利影院在线免费观看| 国产二区三区视频在线观看-四虎精品一区二区在线观看-国产中文字幕一区二区视频-精品一区二区三区av在线|